WA-HST Polyolefine Heat Shrink Tube Type X 385

Applications

  • D = Measurement before shrinking
  • d+W = Measurement after shrinking
  • Polyolefine heat shrink tube, with high shrinking rate. Excellent to cover irregular shapes and elements. Few sizes can cover a wide range of diameters.
General Information
Operating Temperature -55 up to +135 °C
Rate of Shrinking 3:1
Shrink Temperature min. 90 °C
Specification UL 224, 125°C; CSA 22.2
Modification of Length after Shrinking ±5%
Properties
Color Black
Rate of Shrinking 3:1
Withstanding Voltage 20 kV/mm
Specific Flow Resistance 1012

Products

Order Code Data­sheet Ø ID
(mm)
Ø ID min.
(mm)
Rate of Shrinking Modification of Length after Shrinking Withstanding Voltage
(kV/mm)
Samples
71201615
0.5 1.5 3:1 ±5% 20
71203215
1 3 3:1 ±5% 20
71206415
2 6 3:1 ±5% 20
71209515
3 9 3:1 ±5% 20
71212715
4 12 3:1 ±5% 20
71219115
6 18 3:1 ±5% 20
71225415
8 24 3:1 ±5% 20
71239015
13 39 3:1 ±5% 20
Order Code Data­sheet
71201615
71203215
71206415
71209515
71212715
71219115
71225415
71239015
Samples
Order Code Data­sheet Ø ID
(mm)
Ø ID min.
(mm)
Rate of Shrinking Modification of Length after Shrinking Withstanding Voltage
(kV/mm)